Treatment of a tear in paper, of stains and of tidelines — pastel after water damage
Water had stained the sheet and weakened it to the point of tearing, at the shoulder.
The photographs






The treatment
Damp stains and a tear in the paper, following water damage. Water had migrated into the sheet: tidelines, foxing and a grayish veil over the blue ground and the flesh tones, and paper weakened to the point of tearing, here at the shoulder.
A pastel is not treated like a painting: nothing holds the color in place. It rests on the grain of the paper alone, and the slightest contact takes it away. The whole treatment is therefore carried out without ever touching the surface — the work is done from the reverse, the sheet laid flat, the gesture guided with tweezers under the binocular microscope.
The tear is closed from the reverse, fiber by fiber. The stains are drawn out gradually, by indirect contact and controlled drying, without ever wetting the colored surface.
A pastel is never fixed. A fixative would make the surface more stable, but it would extinguish the velvety bloom that is the whole point of the technique — precisely what the artist was after. The background recovers its blue, the skin its light, and the work keeps its powder.
In brief
- Material
- Pastel and paper
- Condition treated
- Water damage
- Place
- À L’Atelier, 28 rue Traversière, Paris 12ᵉ
The condition report and the estimate are free of charge at À L’Atelier and commit you to nothing. One call is enough to find out what can be done.